MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Akrochem RETARDER SAX
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: Retarder SAX is composed of 90% technical salicylic acid/ 10% light paraffinic oil and is utilized as a vulcanization inhibitor for SBR and Natural Rubber compounds. It is especially effective with thioazole, thiazoline and thiuram accelerator systems to prevent scorching at processing temperatures. The recommended level of usage is approximately 0.5 - 1.0 phr. A slight phr adjustment may be necessary to achieve the desired processing safety. Retarder SAX also slows reversion of natural rubber compounds. Retarder SAX is also recommended as an accelerator for mercaptan type polychloroprenes (M Bayprens or W Neoprenes). 1-2 phr of Retarder SAX in "gum" of lightly loaded "M" or "W" type polychloroprenes produces vulcanizates with high modulus and high elongation to break. Retarder SAX is also effective in lead press cured mineral filled "M" or "W" type polychloroprenes compounds where sulfur cannot be tolerated. Retarder SAX is not recommended in black filled CR stocks due to potential scorch reductions. SAX will also accelerate the crosslinking of two-step phenolic resins.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.35 g/cc
Ash <= 0.10 %
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.20 %
 
Descriptive Properties
Appearanceoff-white crystalline powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH579 / 315497

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.