PA6 30% glass fiber reinforced, injection molding grade. Heat stabilization, very high flow ability. Black color. Suitable for parts requiring superior surface aspect quality. Due to its outstanding high flow characteristics this grade provides productivity improvement and more freedom in part design. Information provided by Radici Group. |