MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Wolf Kunststoff INKUFORM LC H5W
Categories: Polymer; Thermoplastic

Material Notes:

Information provided by Wolf Kunststoff

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A >= 100DIN 53505
Hardness, Shore D 81DIN 53505
Ball Indentation Hardness 119 MPaH358/30; DIN 2039
Tensile Strength, Yield 62.0 MPaDIN EN ISO 527
Elongation at Break 14 %DIN EN ISO 527
Elongation at Yield 9.0 %DIN EN ISO 527
Tensile Modulus 2550 MPaDIN EN ISO 527
K Factor (ISO) 0.93 µm/km
@Temperature 20.0 °C
 0.95 µm/km
@Temperature 100 °C
Charpy Impact Unnotched 7.10 kJ/m²EN ISO 179/1eU
Charpy Impact, Notched 6.40 kJ/m²EN ISO 179/1eA
Coefficient of Friction, Dynamic 0.10
@Temperature 20.0 °C
 0.10
@Temperature 100 °C
Coefficient of Friction, Static 0.12
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 120 µm/m-°C
@Temperature 100 °C
ISO E 830
Specific Heat Capacity 1.50 J/g-°C
Thermal Conductivity 0.310 W/m-KDIN 52612
Melting Point 170 °C
Maximum Service Temperature, Air 50.0 °Cfor bushings when pressed
 80.0 °Clong term; UL 746B
 110 °C3 h
Deflection Temperature at 1.8 MPa (264 psi) 105 °CDIN EN ISO 75
Glass Transition Temp, Tg -70.0 °C
Flammability, UL94 HB
@Thickness 3.20 mm
 
Descriptive Properties
Alignment adjustment4Nominal Scale: 1, low; 10, high
Chemical sterilizationNot applicable
ColorWhite
Dimensional stability with moisture absorption3Nominal Scale: 1, low; 10, high
Dimensional stability with temperature variation5Nominal Scale: 1, low; 10, high
Free from PTFEApplicable
Free from siliconeApplicable
Gamma-rays radiation sterilizationNot applicable
Injection molded partsApplicable
Moist heat sterilizationNot applicable
Plastic granulesApplicable
Resistance against dust, dirt, abrasive substances5Nominal Scale: 1, low; 10, high
Resistance to chemicals5Nominal Scale: 1, low; 10, high
Resistant against disinfectantNot applicable
ROHS / WEEEApplicable
Suitable for use in waterNot applicable
Suitable for vacuumNot applicable
UV-sterilizationNot applicable

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PZEDEX3013 / 250070

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.