MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Versalis Revive® COM70HF1 Recycled High Density Polyethylene
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Versalis Revive® PE COM70HF1 is a HDPE based polyolefin compound containing 70% of post-consumer plastic from municipal waste separate collection, stabilizers and compatibilizers agents, allowing its use in high content technological applications.

Applications: COM70HF1 is indicated for the production of extruded packaging and manufactured articles for which sustainability is a primary value. COM70HF1 is suitable to be transformed with blown film technology. It is preferably to be used in coextrusion, in one or more internal layers and in a mixture with virgin polyethylene for the production of industrial packaging products, tubes and various profiles. The percentages of use (up to 100%) and the thicknesses must be assessed according to the final characteristics of the application. The product is not suitable for the production of articles and materials intended for direct contact with food and pharmaceutical and / or medical applications.

Typical properties of an extruded film 180 °C - 210 ° C, BUR 4 and thickness 50 micron.

Information provided by Versalis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.950 g/ccBase resin density; ISO 1183
Thickness 50.0 micronsAs Tested
 20.0 - 100 microns
Melt Flow 1.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 95 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 450 %ISO 527-3
Film Elongation at Break, TD 500 %ISO 527-3
Elmendorf Tear Strength, MD 1.00 g/micronISO 6383-2
Elmendorf Tear Strength, TD 2.00 g/micronISO 6383-2
Dart Drop Test 90.0 gF50; ISO 7765-1/A
Film Tensile Strength at Break, MD 40.0 MPaISO 527-3
Film Tensile Strength at Break, TD 40.0 MPaISO 527-3
1% Secant Modulus, MD 650 MPaISO 527-3
1% Secant Modulus, TD 800 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 135 °CManufacturer method
Vicat Softening Point 128 °C
@Load 1.00 kg
ISO 306/A
Brittleness Temperature <= -60.0 °CASTM D 746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENF9844 / 265665

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.