Pharmalene MP 31 PH is a medium fluidity low density polyethylene resin (LDPE) with slip agent and anti-block obtained by high pressure autoclave process. It is produced according to good manufacturing practices (GMP) and is mainly used for injection molding. Application: Pharmalene MP 31 PH is intended for the use within pharmaceutical sector and is characterized by a good balance between flow ability and rigidity. Pharmalene MP 31 PH is suitable for the production of syringes and caps & closures. Information provided by Versalis. |