System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC LNP™ COLORCOMP™ Compound D1000RXP Polycarbonate (PC)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
Material Notes:
LNP COLORCOMP D1000RXP compound is based on Polycarbonate (PC) resin. Added features of this grade include: Mold Release.
Features: Aesthetics and Appearance,Custom Color,Good Mold Release
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.20
g/cc
ASTM D792
1.205
g/cc
ASTM D792
Density
1.19
g/cc
ASTM D792
Water Absorption
0.15 %
@Time 86400 sec
ASTM D570
Moisture Absorption
0.0200 %
Injection Molding
Moisture Absorption at Equilibrium
0.58 %
@Temperature 100 °C
ASTM D570
Water Absorption at Saturation
0.35 %
ASTM D570
Linear Mold Shrinkage, Flow
0.0050
-
0.0070
cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow
7.0
g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Rockwell M
70
ASTM D785
Hardness, Rockwell R
118
ASTM D785
Tensile Strength at Break
68.0
MPa
50 mm/min; ASTM D638
Tensile Strength, Yield
62.0
MPa
50 mm/min; ASTM D638
Elongation at Break
135 %
50 mm/min; ASTM D638
Elongation at Yield
7.0 %
50 mm/min; ASTM D638
Flexural Strength
97.0
MPa
yld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus
2340
MPa
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched
907
J
ASTM D256
Izod Impact, Unnotched
3204
J/m
ASTM D4812
Tensile Impact Strength
630
kJ/m²
ASTM D1822
Dart Drop, Total Energy
169
J
ASTM D3029
Taber Abrasion, mg/1000 Cycles
10
CS-17, 1 kg; ASTM D1044
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
1.00e+17
ohm-cm
ASTM D257
Dielectric Constant
2.96
@Frequency 1e+6 Hz
ASTM D150
3.17
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength
14.9
kV/mm
@Thickness 3.20 mm
in air; ASTM D149
Dissipation Factor
0.00090
@Frequency 50.0 - 60.0 Hz
ASTM D150
0.010
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index
250
-
400
V
UL 746A
Hot Wire Ignition, HWI
30
-
60
sec
UL 746A
15
-
30
sec
@Thickness >=1.10 mm
UL 746A
30
-
60
sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI
30
-
60
arcs
@Thickness >=1.10 mm
UL 746A
60
-
120
arcs
@Thickness >=3.00 mm
UL 746A
>=
120
arcs
@Thickness >=1.50 mm
UL 746A
Thermal Properties
Original Value
Comments
CTE, linear, Parallel to Flow
68.4
µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
Specific Heat Capacity
1.25
J/g-°C
ASTM C351
Thermal Conductivity
0.290
W/m-K
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi)
137
°C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
132
°C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point
154
°C
Rate B/50; ASTM D1525
UL RTI, Electrical
130
°C
UL 746B
UL RTI, Mechanical with Impact
130
°C
UL 746B
UL RTI, Mechanical without Impact
130
°C
UL 746B
Flammability, UL94
HB
@Thickness >=0.700 mm
UL 94
Optical Properties
Original Value
Comments
Refractive Index
1.586
ASTM D542
Haze
1.0 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible
88 %
@Thickness 2.54 mm
ASTM D1003
Processing Properties
Original Value
Comments
Nozzle Temperature
305
-
325
°C
Zone 2
300
-
320
°C
Zone 3
310
-
330
°C
Melt Temperature
310
-
330
°C
Injection Molding
Mold Temperature
80.0
-
115
°C
Drying Temperature
120
°C
Injection Molding
Dry Time
3.00
-
4.00
hour
Injection Molding
48.0
hour
Cumulative; Injection Molding
Back Pressure
0.300
-
0.700
MPa
Shot Size
40 - 60 %
Vent Depth
0.00250
-
0.00760
cm
Screw Speed
40
-
70
rpm
Descriptive Properties
UV-light, water exposure/immersion
F2
UL 746C
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABH80539 / 288486
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.