LNP THERMOTUF WF009N compound is based on Polybutylene Terephthalate (PBT) resin containing 45% glass fiber. Added features of this grade include: Impact Modified, Good Metal Bonding Strength and Good Chemical Resistance suitable for Nano-Molding Technology (NMT) applications. Features: Impact Modified,High Stiffness,Chemical Resistance,Good metal adhesion,Nano molding technology grade,High Impact Resistance,Structural Information provided by SABIC |