MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond Supreme 45HT-3 Two component, quartz filled epoxy system
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • Very long open time
  • High temperature resistance
  • Exceptional compressive strength
  • Withstands abrasive forces
Product Description: Master Bond Supreme 45HT-3 is a two component, toughened epoxy system for high performance bonding, sealing and casting. It has a forgiving 100 to 15 mix ratio by weight. The working life after mixing is 12-24 hours and it provides moderate to high viscosity with good flow. The system requires oven curing at 250°F for 6 to 8 hours, or 4 to 6 hours at 350°F. The optimal cure schedule is 300°F for 2 to 3 hours, followed by a post cure at 350°F for 4 to 6 hours. It is 100% reactive without any solvents or diluents. Supreme 45HT-3 has very low linear as well as volumetric shrinkage upon curing. Supreme 45HT-3 bonds well to a wide variety of substrates, including metals, composites, ceramics and many different plastics. After curing, it has a number of desirable physical strength properties including a high modulus and exceptional compressive strength. It is a toughened system that can withstand rigorous thermal cycling. This epoxy excels in withstanding chemicals seen in downhole environments, be it acids, bases or solvents. The presence of the quartz filler confers enhanced dimensional stability and increased abrasion resistance. Supreme 45HT-3 is a reliable electrical insulator. It is a relatively high Tg epoxy with a service temperature range from -100°F to +550°F. The color of Part A is tan and Part B is brown. Everything considered, Supreme 45HT-3 is a versatile system that can be used in aerospace, electronic, oil and chemical processing, specialty OEM, and similar type applications.

Product Advantages:

  • Long working life
  • Low linear and volumetric shrinkage upon curing
  • Extremely chemical resistant
  • High glass transition temperature
  • Impressive compressive strength
  • Robust dimensional stability

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 500 - 2500 cP500 - 2500 cPPart B
 50000 - 100000 cP50000 - 100000 cPMixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 80 - 9080 - 90
Tensile Strength 62.1 - 68.9 MPa9000 - 10000 psi
Tensile Modulus 3.79 - 4.14 GPa550 - 600 ksi
Compressive Strength 165 - 179 MPa24000 - 26000 psi
Adhesive Bond Strength 15.2 - 16.5 MPa2200 - 2400 psiTensile lap shear, Al to Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 4.5
@Frequency 60 Hz
4.5
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 30.0 - 35.0 µm/m-°C16.7 - 19.4 µin/in-°F
Maximum Service Temperature, Air 288 °C550 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
Glass Transition Temp, Tg 145 - 155 °C293 - 311 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 149 °C
2.00 - 3.00 hour
@Temperature 300 °F
Optimum, with a post cure at 350°F for 4-6 hours
 240 - 360 min
@Temperature 177 °C
4.00 - 6.00 hour
@Temperature 350 °F
 360 - 480 min
@Temperature 121 °C
6.00 - 8.00 hour
@Temperature 250 °F
Working Life 720 - 1440 min720 - 1440 minafter mixing, 100 gram batch
Shelf Life 6.00 Month6.00 Monthin original, unopened containers
 
Descriptive Properties
Mixing ratio100:15 by weightParts A to B
ViscositypastePart A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMASTM5942 / 306831

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.