MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin SE1X Polyphenylene Ether + PS (PPE+PS) (Asia)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ SE1X resin is a non-reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant and carries a UL94 flame rating of V0/V1 at 1.5mm along with a UL746C Outdoor Suitability rating of F1. NORYL SE1X resin offers strong electrical performance, low moisture absorption, dimensional stability, and hydrolytic stability. This material is an excellent candidate for indoor and outdoor electrical enclosures , heating ventilation / air conditioning (HVAC) applications, and solar / photovoltaic (PV) junction box applications. *for enhanced processing version, please see NORYL NH5120 resin grade.

Features: Weatherable,Non-Halogenated,Non-Chlorinated,Non-Brominated

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccASTM D792
Water Absorption 0.060 %
@Time 86400 sec
ASTM D570
Moisture Absorption 0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 53.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 65.0 MPa50 mm/min; ASTM D638
Elongation at Break 15 %50 mm/min; ASTM D638
Elongation at Yield 4.0 %50 mm/min; ASTM D638
Flexural Strength 100 MPayld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 2400 MPa2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 180 JASTM D256
 106 J
@Temperature -30.0 °C
ASTM D256
Dart Drop, Total Energy 51.0 Jpeak; ASTM D3763
 32.0 J
@Temperature -30.0 °C
peak; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.30e+16 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmASTM D257
Dielectric Constant 2.46
@Frequency 1e+6 Hz
ASTM D150
 2.52
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 18.1 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
Dissipation Factor 0.0021
@Frequency 1e+6 Hz
ASTM D150
 0.0034
@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 60 - 120 secASTM D495
Comparative Tracking Index 400 - 600 VUL 746A
Hot Wire Ignition, HWI >= 120 sec
@Thickness >=1.50 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=1.50 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 126 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 118 °C
@Thickness 6.40 mm
unannealed; ASTM D648
UL RTI, Electrical 110 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 110 °CUL 746B
Flammability, UL94 V-1
@Thickness >=1.50 mm
UL 94
 V-0
@Thickness >=6.00 mm
UL 94
Glow Wire Ignition Temperature 700 °C
@Thickness 1.00 mm
IEC 60695-2-13
 700 °C
@Thickness 1.50 mm
IEC 60695-2-13
 725 °C
@Thickness 2.00 mm
IEC 60695-2-13
 725 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 900 °C
@Thickness 1.00 mm
IEC 60695-2-12
 900 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 280 - 310 °C
Zone 2 260 - 305 °C
Zone 3 270 - 310 °C
Melt Temperature 280 - 310 °CInjection Molding
Mold Temperature 75.0 - 105 °C
Drying Temperature 105 - 110 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 70 %
Screw Speed 20 - 100 rpm
 
Descriptive Properties
Radiant Panel ListingRP100UL Tested
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82475 / 290422

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.