This PTFE, reinforced with carbon fibres, has a particularly low coefficient of friction and high wear resistance, particularly in wet running conditions. This grade is also suitable for non-hardened friction partners, has good mechanical property values, excellent flexibility, and good chemical resistance, and is heat- dissipating.Information provided by Angst + Pfister |