System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
SABIC LNP™ LUBRICOMP™ Compound RP004 Polyamide 66 (Nylon 66) (Asia)
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 66 (PA66)
Material Notes:
LNP LUBRICOMP RP004 compound is based on Nylon 6/6 resin containing 20% PTFE/silicone. Added features of this grade include: Wear Resistant.
Features: Wear resistant
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.24
g/cc
0.0448
lb/in³
ASTM D792
1.24
g/cc
0.0448
lb/in³
ISO 1183
Moisture Absorption
0.800 %
0.800 %
23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow
0.019
cm/cm
0.019
in/in
24hrs; ASTM D955
0.019
cm/cm
0.019
in/in
24hrs; ISO 294
Linear Mold Shrinkage, Transverse
0.019
cm/cm
0.019
in/in
24hrs; ASTM D955
0.019
cm/cm
0.019
in/in
24hrs; ISO 294
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
60.0
MPa
8700
psi
ASTM D638
63.0
MPa
9140
psi
ISO 527
Tensile Strength, Yield
63.0
MPa
9140
psi
ISO 527
Elongation at Break
22.5 %
22.5 %
ASTM D638
26.6 %
26.6 %
ISO 527
Elongation at Yield
22 %
22 %
ASTM D638
26 %
26 %
ISO 527
Tensile Modulus
2.73
GPa
396
ksi
1 mm/min; ISO 527
2.75
GPa
399
ksi
50 mm/min; ASTM D638
Flexural Strength
82.0
MPa
11900
psi
ISO 178
Flexural Modulus
2.00
GPa
290
ksi
ISO 178
2.06
GPa
299
ksi
ASTM D790
Izod Impact Notched
53.0
J
39.1
ft-lb
ASTM D256
Izod Impact, Unnotched
3.47
J/cm
6.50
ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO)
5.00
kJ/m²
2.38
ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
88.0
kJ/m²
41.9
ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy
6.00
J
4.43
ft-lb
peak; ASTM D3763
Impact Test
1.00
J
0.738
ft-lb
Multiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic
0.19
0.19
ASTM D3702 Modified: Manual
Coefficient of Friction, Static
0.040
0.040
ASTM D3702 Modified: Manual
K (wear) Factor
6.04
x 10
-8
mm³/N-M
3.00
x 10
-10
in³-min/ft-lb-hr
Washer; ASTM D3702 Modified: Manual
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
82.8
µm/m-°C
@Temperature -40.0 - 40.0 °C
46.0
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
84.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
46.7
µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow
93.6
µm/m-°C
@Temperature -40.0 - 40.0 °C
52.0
µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
94.0
µm/m-°C
@Temperature -40.0 - 40.0 °C
52.2
µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi)
200
°C
392
°F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
237
°C
@Thickness 3.20 mm
459
°F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
63.0
°C
145
°F
Flatw 80*10*4 sp=64mm; ISO 75/Af
63.0
°C
@Thickness 3.20 mm
145
°F
@Thickness 0.126 in
unannealed; ASTM D648
UL RTI, Electrical
65.0
°C
149
°F
UL 746B
UL RTI, Mechanical with Impact
65.0
°C
149
°F
UL 746B
UL RTI, Mechanical without Impact
65.0
°C
149
°F
UL 746B
Flammability, UL94
HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
UL 94
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PSABH81037 / 288984
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.