MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC 324CN Linear Low Density Polyethylene for Wire & Cable  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Product Description: 324CN is a Linear Low Density Polyethylene natural resin for wire and cable applications. It contains a low level of antioxidants and does not contain any slip or antiblock additives. Sufficient antioxidant and Cu-inhibitor should be added to meet specific ageing requirements. For jacketing applications, addition of Carbon Black or UV stabilizer is required.

Typical Applications: One-step or two-step Silane cross-linkable insulation for Low Voltage power insulation cable, Aerial bundle cable, also suitable for telecommunication and Low Voltage power cable jacketing.

Information provided by SABIC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccload density; ASTM D1505
Melt Flow 3.6 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 53ASTM D2240
Tensile Strength at Break 18.0 MPaASTM D638
Tensile Strength, Yield 11.0 MPaASTM D638
Elongation at Break 600 %ASTM D638
Elongation at Yield 14 %ASTM D638
1% Secant Modulus 225 MPaASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.40e+18 ohm-cmat 500 V; ASTM D257
Dielectric Constant 2.28
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 37.0 kV/mm1000 V/sec; ASTM D149
Dissipation Factor 0.00043
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Melting Point 121 °CPeak; SABIC Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
SABIC 318CN Linear Low Density Polyethylene for Wire & Cable
NOVA Chemicals Novapol® PF-Y821-BP Butene LLDPE Film Resin
LyondellBasell Petrothene® GA501020 Linear Low Density Polyethylene
NOVA Chemicals Novapol® PF-Y821-CP Butene LLDPE Film Resin
NOVA Chemicals Novapol® PF-0118-C Butene LLDPE Film Resin

PSABICZ840 / 133036

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.