MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Amodel® A-4122 NL WH 905 PPA, 22% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 20% Glass Fiber Reinforced

Material Notes: 22% glass fiber, high-reflectivity white for LEDs, fast cycle time, hot-water molds

Amodel® A-4122 NL resin is a 22% glass reinforced, high-reflectivity white grade of polyphthalamide (PPA), designed to provide high crystallinity when molded in water-cooled molds. This material exhibits high heat resistance, high strength and stiffness over a broad temperature range. It also offers low moisture absorption, excellent chemical resistance and excellent electrical properties.

Its rapid crystallization rate and high flow can result in short cycles and therefore high molding productivity and lower part cost.

- White: A-4122 NL WH 905

Markets/Uses: Automotive / Automotive E/E / LEDs

Applications: Automotive Applications; Automotive Electronics; Automotive Under the Hood; Electrical/Electronic Applications

Features: Chemical Resistant; Fast Molding Cycle; Good Color Stability; High Reflectivity; High Stiffness; Low Moisture Absorption

Injection notes: A general purpose screw is recommended, with minimum back pressure.
Injection Pressure: 3 to 4 in/sec
Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.48 g/cc0.0535 lb/in³Method A; ISO 1183
Water Absorption 0.24 %
@Time 86400 sec
0.24 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cm0.0060 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 124124ASTM D785
Tensile Strength at Break 123 MPa17800 psiASTM D638
Elongation at Break 1.6 %1.6 %ASTM D638
Tensile Modulus 9.17 GPa1330 ksiASTM D638
Flexural Yield Strength 171 MPa24800 psiASTM D790
Flexural Modulus 8.00 GPa1160 ksiASTM D790
Izod Impact, Notched 0.270 J/cm0.506 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  11.0 µm/m-°C
@Temperature 150 - 250 °C
6.11 µin/in-°F
@Temperature 302 - 482 °F
ASTM E831
 23.0 µm/m-°C
@Temperature 0.000 - 100 °C
12.8 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM E831
CTE, linear, Transverse to Flow  86.0 µm/m-°C
@Temperature 0.000 - 100 °C
47.8 µin/in-°F
@Temperature 32.0 - 212 °F
ASTM E831
 130 µm/m-°C
@Temperature 150 - 250 °C
72.2 µin/in-°F
@Temperature 302 - 482 °F
ASTM E831
Melting Point 324 °C615 °FPeak; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 313 °C595 °FUnannealed; ASTM D648
 
Optical PropertiesMetricEnglishComments
Reflection Coefficient, Visible (0-1) 0.900.90ASTM E1331
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 318 - 324 °C604 - 615 °F
Front Barrel Temperature 327 - 332 °C621 - 630 °F
Melt Temperature 329 - 343 °C624 - 649 °FInjection
Mold Temperature 66.0 - 93.0 °C151 - 199 °F
Drying Temperature 120 °C
@Time 14400 sec
248 °F
@Time 4.00 hour
Moisture Content 0.030 - 0.060 %0.030 - 0.060 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorWhite
FormsPellets
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4052 / 279852

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.