MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC LNP™ ELCRIN™ WF006NiQ2 Polybutylene Terephthalate (PBT)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: LNP ELCRIN WF006NiQ2 compound is based on Polybutylene terephthalate (PBT) resin utilizing ELCRIN iQ 2nd generation upcycling technology and containing 30% glass fiber. Added features of this grade includes: Minimum 25% PCR weight content, High Flow, High Metal Bonding Strength and Good Chemical Resistance.

Features: Post-Consumer Recycled (PCR) content,High Stiffness,Chemical Resistance,Good metal adhesion,Nano molding technology grade,High Flow,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.49 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
Viscosity 15 cP
@Load 5.00 kg,
Temperature 250 °C
MVR cc/10 min; ISO 1133
 23 cP
@Load 5.00 kg,
Temperature 270 °C
MVR cc/10 min; ISO 1133
 29 cP
@Load 5.00 kg,
Temperature 275 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0050 cm/cmSABIC method
Melt Flow 21 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 37 g/10 min
@Load 5.00 kg,
Temperature 275 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPa5 mm/min; ASTM D638
 111 MPa5 mm/min; ISO 527
Elongation at Break 2.5 %5 mm/min; ASTM D638
 2.5 %5 mm/min; ISO 527
Tensile Modulus 8600 MPa1 mm/min; ISO 527
 8760 MPa5 mm/min; ASTM D638
Flexural Strength 168 MPabreak, 2mm/min; ISO 178
 170 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 7100 MPa2 mm/min; ISO 178
 7700 MPa1.3 mm/min, 50 mm span; ASTM D790
Adhesive Bond Strength 33.0 MPa("T" treatment, shear type); ISO 19095
Izod Impact Notched 137 JASTM D256
 100 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 870 J/mASTM D4812
Izod Impact, Notched (ISO) 13.0 kJ/m²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 54.0 kJ/m²80*10*4; ISO 180/1U
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.53
@Frequency 1e+10 Hz
SABIC method
 3.59
@Frequency 5.00e+9 Hz
SABIC method
 3.61
@Frequency 1.10e+9 Hz
SABIC method
 3.62
@Frequency 1.90e+9 Hz
SABIC method
Dissipation Factor 0.0090
@Frequency 1e+10 Hz
SABIC method
 0.010
@Frequency 5.00e+9 Hz
SABIC method
 0.012
@Frequency 1.90e+9 Hz
SABIC method
 0.013
@Frequency 1.10e+9 Hz
SABIC method
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 23.0 µm/m-°C
@Temperature 23.0 - 50.0 °C
ISO 11359-2
 23.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 24.0 µm/m-°C
@Temperature 23.0 - 50.0 °C
ASTM E831
 24.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 81.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 86.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 90.0 µm/m-°C
@Temperature 23.0 - 50.0 °C
ASTM E831
 96.0 µm/m-°C
@Temperature 23.0 - 50.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 200 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 204 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 156 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 162 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 245 - 275 °C
Zone 2 250 - 270 °C
Zone 3 250 - 270 °C
Melt Temperature 250 - 270 °CInjection Molding
Mold Temperature 140 - 160 °C
Drying Temperature 100 - 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Precipitation Temperature 40.0 - 60.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80620 / 288567

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.