LNP LUBRICOMP WAL34I compound is based on Polybutylene Terephthalate (PBT) resin containing 15% PTFE, 20% aramid fiber. Added features of this grade include: Internally Lubricated, Wear Resistant, Impact Modified Features: Internally Lubricated,Wear resistant Information provided by SABIC |