LNP COLORCOMP W10009I compound is based on Polybutylene Terephthalate (PBT) resin. Added features of this grade include: Flame Retardant, Impact Modified. Features: Impact Modified,Aesthetics and Appearance,Custom Color,Flame Retardant Information provided by SABIC |