MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ FARADEX™ Compound NS003 Polycarbonate + ABS (PC+ABS)
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced

Material Notes: LNP FARADEX NS003 compound is based on Polycarbonate/Acrylonitrile Butadiene Styrene (PC/ABS) blend containing 15% stainless steel fiber. Added features of this grade include: Electrically Conductive, EMI/RFI shielding.

Features: EMI/RFI Shielding,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.21 g/ccISO 1183
 1.24 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
 0.100 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm24hrs; ASTM D955
 0.0030 cm/cm24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0035 cm/cm24hrs; ASTM D955
 0.0035 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 46.0 MPaISO 527
 49.0 MPaASTM D638
Tensile Strength, Yield 50.0 MPaISO 527
 52.0 MPaASTM D638
Elongation at Break 4.7 %ASTM D638
 6.0 %ISO 527
Elongation at Yield 3.3 %ASTM D638
 3.5 %ISO 527
Tensile Modulus 2700 MPa1 mm/min; ISO 527
 3100 MPa50 mm/min; ASTM D638
Flexural Strength 86.0 MPaISO 178
 89.0 MPaASTM D790
Flexural Modulus 2800 MPaISO 178
 2990 MPaASTM D790
Izod Impact Notched 74.0 JASTM D256
Izod Impact, Unnotched 573 J/mASTM D4812
Izod Impact, Notched (ISO) 9.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 32.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 15.0 Jpeak; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10000 ohm-cmASTM D257
Surface Resistance 10 - 1000 ohmASTM D257
Static Decay <= 0.010 sec5000V to <50V; FTMS101B
Shielding Effectiveness 50 - 65 dB
@Thickness 3.00 mm
SABIC method
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 59.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 63.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 77.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 82.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 115 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 120 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 103 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 105 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 230 - 245 °C
Zone 3 245 - 255 °C
Melt Temperature 220 - 260 °CInjection Molding
Mold Temperature 40.0 - 80.0 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80632 / 288579

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.