MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ THERMOCOMP™ Compound UX08319 Polyphthalamide (PPA)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: LNP THERMOCOMP UX08319 compound is based on Polyphthalamide (PPA) resin containing 30% glass fiber. Added features of this grade include: Improved Plating Surface and Mechanical Performance suitable for Laser Direct Structuring (LDS) applications, Improved Dielectric Properties.

Features: High Stiffness,Laser Direct Structuring,Dielectrics,Circuit Solution,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.14 g/cc0.0773 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0033 cm/cm0.0033 in/inSABIC method
Linear Mold Shrinkage, Transverse 0.0035 cm/cm0.0035 in/inSABIC method
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 125 MPa18100 psi5 mm/min; ASTM D638
Elongation at Break 1.4 %1.4 %5 mm/min; ASTM D638
Tensile Modulus 13.784 GPa1999.2 ksi5 mm/min; ASTM D638
Flexural Strength 185 MPa26800 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 11.5 GPa1670 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 40.0 J29.5 ft-lbASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 6.2
@Frequency 1.90e+9 Hz
6.2
@Frequency 1.90e+9 Hz
SABIC method
Dissipation Factor 0.015
@Frequency 1.90e+9 Hz
0.015
@Frequency 1.90e+9 Hz
SABIC method
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 265 °C
@Thickness 3.20 mm
509 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 310 - 330 °C590 - 626 °F
Zone 3 300 - 330 °C572 - 626 °F
Melt Temperature 315 - 330 °C599 - 626 °FInjection Molding
Mold Temperature 140 - 165 °C284 - 329 °F
Drying Temperature 120 - 130 °C248 - 266 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Back Pressure 20.0 - 40.0 MPa2900 - 5800 psi
Screw Speed 30 - 70 rpm30 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81943 / 289890

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.