MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ascend Performance Materials Vydyne® 22HSP NT Nylon 66, Heat Stabilized, Conditioned  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes:

Availability:

  • Asia Pacific
  • Europe
  • North America
Additive:
  • Lubricant
  • Heat Stabilizer
Features:
  • Fast Molding Cycle
  • Gasoline Resistance
  • General Purpose
  • Good Abrasion Resistance
  • Good Chemical Resistance
  • Good Mold Release
  • Good Toughness
  • High Rigidity
  • High Strength
  • Lubricated
  • Oil Resistant
  • Solvent Resistant
Uses:
  • Bearings
  • Bushings
  • Cams
  • Connectors
  • Housings
  • Industrial Applications
Appearance: Natural Color

Forms: Pellets

Processing Method: Injection Molding

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³ISO 1183
Water Absorption 1.2 %
@Time 86400 sec
1.2 %
@Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 2.4 %2.4 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.022 cm/cm
@Diameter 2.00 mm
0.022 in/in
@Diameter 0.0787 in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.020 cm/cm
@Diameter 2.00 mm
0.020 in/in
@Diameter 0.0787 in
ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 40.0 MPa5800 psiISO 527-2
Tensile Strength, Yield 55.0 MPa7980 psiISO 527-2
Elongation at Break >= 50 %>= 50 %ISO 527-2
Elongation at Yield 20 %20 %ISO 527-2
Tensile Modulus 1.80 GPa261 ksiISO 527-2
Flexural Strength 30.0 MPa4350 psiISO 178
Flexural Modulus 1.00 GPa145 ksiISO 178
Izod Impact, Notched (ISO)  7.00 kJ/m²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 180
 20.0 kJ/m²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wellman Wellamid® 22L-N Unfilled Nylon 66, Lubricated
Wellman Wellamid® 22LH-WBK Unfilled Nylon 66
Wellman Wellamid® 22LH-NBK4/WE1657 Unfilled Nylon 66
Wellman Wellamid® 22LH-NBK4 Unfilled Nylon 66
Wellman Wellamid® 21LH-NBK4 General Purpose Nylon 66

PVYDYM816 / 177167

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.