MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Mitsubishi ROLASERIT® PBT01 PBT 3D Printing Powder
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: High Performance Polymer for Powder Bed Fusion Applications

Features:

  • Easy flowing
  • Works on SLS and all other standard Powder Bed Fusion machines
  • Only single laser exposure
  • High ductility
  • Low warpage
  • No additional additives are necessary
Colors: ROLASERIT is available in Natural/white

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccPart-Density, z-direction; ISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 45.0 MPaz-direction; ISO 527
 49.0 MPaxy-plane; ISO 527
Elongation at Break 4.5 %z-direction; ISO 527
 15 %xy-plane; ISO 527
Tensile Modulus 2450 MPa(E), z-direction; ISO 527
 2650 MPa(E), xy-plane; ISO 527
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 108 °Cz-direction
Deflection Temperature at 0.46 MPa (66 psi) 133 °Cz-direction; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °Cz-direction; ISO 75-1/-2
 
Descriptive Properties
AppearanceFinest Powder Natural color

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMITS9846 / 301071

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.