Nexeo® HIVAL® PE HD 506060 HDPE
Categories:
Polymer
;
Thermoplastic
;
Polyethylene (PE)
;
High Density (HDPE)
;
High Density Polyethylene (HDPE), Blow Molding Grade
Material Notes:
Food Contact Acceptable; High Density
Agency Ratings: FDA 21 CFR 177.1520
Forms: Pellets
Processing Method: Blow Molding
Information provided by Nexeo® Solutions.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
0.965
g/cc
0.0349
lb/in³
ASTM D1505
Melt Flow
8.5
g/10 min
@Load 2.16 kg,
Temperature 190 °C
8.5
g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Tensile Strength, Yield
30.3
MPa
4390
psi
ASTM D638
Elongation at Yield
6.0 %
6.0 %
ASTM D638
Flexural Modulus, 1% Secant
1520
MPa
220000
psi
ASTM D790
Izod Impact, Notched
0.590
J/cm
1.11
ft-lb/in
ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
82.2
°C
180
°F
Unannealed; ASTM D648
Compliance Properties
Metric
English
Comments
FDA
Yes
Yes
Descriptive Properties
Availability
North America
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PNEXEO815 / 316347
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.