MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
DuPont Silastic® Q7-4780 Dow-Corning Biomedical Grade ETR Elastomer  (Unverified Data**)
Categories: Polymer; Thermoset; Silicone

Material Notes:

Information provided by Multibase

Former Dow (Multibase) grade.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccas molded- 10 minutes at 116°C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 76as molded- 10 minutes at 116°C
 83post cured- 2 hours at 177°C
 83post cured- 4 hours at 177°C
 84post cured- 8 hours at 177°C
Tensile Strength, Ultimate 876 psipost cured- 8 hours at 177°C
 970 psipost cured- 4 hours at 177°C
 1010 psipost cured- 2 hours at 177°C
 1111 psias molded- 10 minutes at 116°C
Tensile Strength, Yield 548 psiat 200%, as molded- 10 minutes at 116°C
 597 psiat 200%, post cured- 2 hours at 177°C
 606 psi200%, post cured- 4 hours at 177°C
 611 psi200%, post cured- 8 hours at 177°C
Elongation at Break 384 %post cured- 8 hours at 177°C
 444 %post cured- 4 hours at 177°C
 483 %post cured- 2 hours at 177°C
 654 %as molded- 10 minutes at 116°C
Tear Strength 122 plipost cured- 8 hours at 177°C; Die B
 129 plipost cured- 4 hours at 177°C; Die B
 150 plipost cured- 2 hours at 177°C; Die B
 243 plias molded- 10 minutes at 116°C; Die B
Compression Set 62.5 %22 hours at 177°C, post cured- 4 hours at 177°C
 70.9 %22 hours at 177°C, as molded-10 minutes at 116°C
 73.4 %22 hours at 177°C, post cured- 8 hours at 177°C
 81.2 %22 hours at 177°C, post cured- 2 hours at 177°C
 
Thermal PropertiesOriginal ValueComments
Shrinkage 1.9 %
@Temperature 116 °C,
Time 601 sec
as molded
 2.3 %
@Temperature 177 °C,
Time 7200 sec
post cured
 2.4 %
@Temperature 177 °C,
Time 14400 sec
post cured
 2.7 %
@Temperature 177 °C,
Time 28800 sec
post cured

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Silastic® Q7-4780 BIOMEDICAL GRADE ETR ELASTOMER, KIT
Wacker ELASTOSIL® LR 3016/65 A/B Liquid Silicone Rubber
Dow Silastic® Q7-4765 BIOMEDICAL GRADE ETR ELASTOMER, KIT

PMULTI155 / 54059

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.