MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC NORYL GTX™ Resin GTX840 Polyphenylene Ether + PA (PPE+Nylon) (Americas)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 840 resin is a 40% glass reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade has high stiffness (flexural modulus 11860 MPa), excellent chemical resistance, and high heat resistance. NORYL GTX GTX840 resin is an excellent candidate for a wide variety of applications including automotive under-the-hood and water management.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/ccASTM D792
Density 1.45 g/cc0.0524 lb/in³ISO 1183
Water Absorption  0.63 %
@Time 86400 sec
0.63 %
@Time 24.0 hour
ASTM D570
 0.63 %
@Time 86400 sec
0.63 %
@Time 24.0 hour
ISO 62-1
Moisture Absorption 0.0700 %0.0700 %Injection Molding
 0.130 %0.130 %23°C/50% RH/24 hrs; ISO 62-4
Moisture Absorption at Equilibrium 0.38 %0.38 %23°C/50% RH; ISO 62-4
Water Absorption at Saturation 1.64 %1.64 %ASTM D570
 1.64 %1.64 %ISO 62-1
Viscosity 13 cP
@Load 5.00 kg,
Temperature 220 °C
13 cP
@Load 11.0 lb,
Temperature 428 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0017 cm/cm0.0017 in/in24hrs; ASTM D955
 0.0017 cm/cm0.0017 in/in24hrs; ISO 294
 0.0024 - 0.0027 cm/cm
@Thickness 3.20 mm
0.0024 - 0.0027 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0099 cm/cm0.0099 in/in24hrs; ASTM D955
 0.0099 cm/cm0.0099 in/in24hrs; ISO 294
 0.0060 - 0.0063 cm/cm
@Thickness 3.20 mm
0.0060 - 0.0063 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 15 g/10 min
@Load 5.00 kg,
Temperature 280 °C
15 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 108108ASTM D785
Tensile Strength at Break 200 MPa29000 psi5 mm/min; ISO 527
 201 MPa29200 psi5 mm/min; ASTM D638
Elongation at Break 2.2 %2.2 %5 mm/min; ASTM D638
 2.4 %2.4 %5 mm/min; ISO 527
Tensile Modulus 12.57 GPa1823 ksi1 mm/min; ISO 527
 13.02 GPa1888 ksi5 mm/min; ASTM D638
Flexural Strength 290 MPa42100 psibrk, 1.3 mm/min, 50 mm span; ASTM D790
 306 MPa44400 psibreak, 2mm/min; ISO 178
Flexural Modulus 11.73 GPa1701 ksi2 mm/min; ISO 178
 11.8 GPa1710 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 114 J84.1 ft-lbASTM D256
 90.0 J
@Temperature -30.0 °C
66.4 ft-lb
@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 10.4 J/cm19.5 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²5.23 ft-lb/in²80*10*4; ISO 180/1A
 11.0 kJ/m²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 70.0 kJ/m²33.3 ft-lb/in²80*10*4; ISO 180/1U
Charpy Impact Unnotched 7.20 J/cm²34.3 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²5.23 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  17.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
9.44 µin/in-°F
@Temperature 73.4 - 140 °F
ASTM E831
 17.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
9.44 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
 16.0 - 20.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
8.89 - 11.1 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
CTE, linear, Transverse to Flow  70.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 140 °F
ISO 11359-2
 70.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 140 °F
ASTM E831
 90.0 - 94.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
50.0 - 52.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 259 °C498 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 259 °C
@Thickness 6.40 mm
498 °F
@Thickness 0.252 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 244 °C471 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 245 °C
@Thickness 6.40 mm
473 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 247 °C477 °FRate B/50; ASTM D1525
 248 °C478 °FRate B/50; ISO 306
 257 °C495 °FRate A/50; ISO 306
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 295 - 315 °C563 - 599 °F
Zone 2 280 - 315 °C536 - 599 °F
Zone 3 290 - 315 °C554 - 599 °F
Melt Temperature 295 - 315 °C563 - 599 °FInjection Molding
Mold Temperature 75.0 - 120 °C167 - 248 °F
Drying Temperature 95.0 - 105 °C203 - 221 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %0.020 %minimum
Back Pressure 0.300 - 1.40 MPa43.5 - 203 psi
Shot Size 30 - 50 %30 - 50 %
Vent Depth 0.00130 - 0.00380 cm0.000512 - 0.00150 in
Screw Speed 20 - 100 rpm20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82151 / 290098

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.