MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Go Yen Chemical GY-TJ-21 High Effective Composite Elastomer
Categories: Polymer; Thermoplastic

Material Notes:

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 0.30 %0.30 %ASTM D570
Linear Mold Shrinkage 0.020 - 0.060 cm/cm0.020 - 0.060 in/inASTM D955
Melt Flow 0.77 g/10 min0.77 g/10 minASTM D1182
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 8585ASTM D785
Tensile Strength 63.7 MPa9250 psiASTM D638
Elongation at Break 5.0 %5.0 %ASTM D638
Flexural Strength 91.0 MPa13200 psiASTM D790
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10 ohm-cm10 ohm-cmASTM D257
Dielectric Constant 3.73.7ASTM D150-647b
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149
Dissipation Factor 0.190.19ASTM D150
 0.500.50ASTM D150-647
 
Thermal PropertiesMetricEnglishComments
Softening Point 102 °C216 °FASTM D1525
Heat Distortion Temperature 90.0 °C194 °FASTM D648
Flammability, UL94 HB
@Thickness 0.0625 mm
HB
@Thickness 0.00246 in
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4911.491ASTM D542
Transmission, Visible 93 - 97 %93 - 97 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN705 / 267013

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.