MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
UPM Formi Formi 3D 20/19 20% Cellulose fiber filled polylactide acid
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyketone; Polyketone, Glass Fiber Reinforced

Material Notes: Material: UPM Formi 3D is cellulose fiber filled plastic composite. Principal ingredients are specially selected cellulose fibers and native polylactide acid.

Applications: UPM Formi 3D grades are suitable for production of 3D printing filaments to be used in Fused Granular Fabrication (FGF).

Environment: UPM Formi 3D is manufactured from renewable cellulose fibers. Material can be recycled or burned for energy. All cellulose fibers are from certificated forests.

Information provided by UPM

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccEN ISO 1183
Melt Flow 16 g/10 min
@Load 10.0 kg,
Temperature 190 °C
granulate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 39.0 MPaISO 527
Elongation at Break 4.0 %ISO 527
Tensile Modulus 3600 MPaISO 527
Charpy Impact Unnotched 20.0 kJ/m²ISO 179-2/1eU
 
Thermal PropertiesOriginal ValueComments
Melting Point 140 - 180 °CPeak; ISO 11357
Glass Transition Temp, Tg 65.0 °CISO 11357
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 200 °C
Drying Temperature 80.0 °C
Dry Time 3.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PUPMF023 / 286831

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.