MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ChenGuang SFN-D Low M.W. PTFE Aqueous Dispersion
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Description: SFN-D is a low molecular weight aqueous dispersion of PTFE. In addition to superior properties typical of PTFE dispersions, SFN-D features low viscosity, good flow performance, and excellent penetration. It can be used along, or be added as an aid into other ordinary PTFE aqueous dispersions, such as PTFE Aqueous Dispersion SFN-1 . Adding SFN-D at 3 - 5 % by weight into SFN-1, for instance, can offer such advantages to coatings as enhanced bonding to base substance, thicker layer with each pass of coating, more glossy and void-free surface, greater resistance to wear and corrosion.

Applications: SFN-D is usually used as an aid to ordinary PTFE dispersions for the applications of impregnating fabric, porous materials and coating metals by processing methods of dip, coating, and spay coating.

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 50 %50 %
Particle Size 0.19 µm0.19 µm
pH 8.0 - 108.0 - 10
Viscosity Measure 3.0 cSt3.0 cStDynamic
Molecular Weight 10000 - 20000 g/mol10000 - 20000 g/mol
 
Descriptive Properties
ColorMilky white liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGU039 / 255638

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.