Vydyne R413J BK0836 is a black, electrically neutral heat stabilized impact-modified, 15% glass-fiber reinforced PA66 resin. R413J BK0836 is designed to produce a light on dark mark using an IR 1064nm laser.Information provided by Ascend Performance Materials. |