MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC LNP™ THERMOCOMP™ Compound PF008QS Polyamide 6 (Nylon 6)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: LNP THERMOCOMP PF008QS compound is based on Nylon 6 resin containing 40% glass fiber. Added features of this grade include: Heat Stabilized, Reduced Moisture.

Features: High Stiffness,Low Moisture Absorption,Heat Stabilized,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.35 g/cc0.0488 lb/in³ASTM D792
 1.35 g/cc0.0488 lb/in³ISO 1183
Moisture Absorption 0.150 - 0.250 %0.150 - 0.250 %Injection Molding
 0.310 %0.310 %23°C/50% RH/24 hrs; ASTM D570
 0.500 %0.500 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in24hrs; ASTM D955
 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in24hrs; ISO 294
Linear Mold Shrinkage, Transverse 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/in24hrs; ASTM D955
 0.0070 - 0.0090 cm/cm0.0070 - 0.0090 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 152 MPa22000 psiASTM D638
 165 MPa23900 psiISO 527
Elongation at Break 3.0 %3.0 %ASTM D638
 3.4 %3.4 %ISO 527
Tensile Modulus 11.6 GPa1680 ksi1 mm/min; ISO 527
 12.2 GPa1770 ksi50 mm/min; ASTM D638
Flexural Strength 244 MPa35400 psiASTM D790
 262 MPa38000 psiISO 178
Flexural Modulus 9.58 GPa1390 ksiASTM D790
 12.0 GPa1740 ksiISO 178
Izod Impact Notched 170 J125 ft-lbASTM D256
Izod Impact, Unnotched 11.05 J/cm20.70 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 17.0 kJ/m²8.09 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 72.0 kJ/m²34.3 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 12.0 J8.85 ft-lbpeak; ASTM D3763
Impact Test 4.00 J2.95 ft-lbMultiaxial Impact; ISO 6603
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  30.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 30.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
17.2 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  55.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
30.9 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 55.6 µm/m-°C
@Temperature -40.0 - 40.0 °C
30.9 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 218 °C
@Thickness 3.20 mm
424 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 201 °C394 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 199 °C
@Thickness 3.20 mm
390 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 2 255 - 265 °C491 - 509 °F
Zone 3 265 - 275 °C509 - 527 °F
Melt Temperature 255 - 275 °C491 - 527 °FInjection Molding
Mold Temperature 80.0 - 95.0 °C176 - 203 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81783 / 289730

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.