MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Copper Alloy, UNS C49100, H02 Temper, Rod, Bar & Wire
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: 1/2 Hard

Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding, Gas Shielded Arc Welding, Butt Weld, Capacity for Being Hot Formed; Fair Suitability – Spot Weld

Typical Uses: Lead-free, dezinfication resistant alloy for potable water components; Plumbing & Pipe Fittings; Plumbing Castings; Potable water valve bodies, faucets, plumbing components

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.75 g/cc0.316 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 58 - 7558 - 75
Tensile Strength >= 345 MPa>= 50000 psi
Tensile Strength, Yield >= 214 MPa>= 31000 psi0.5% Ext
Elongation at Break 16 %16 %
Tensile Modulus 117 GPa17000 ksi
Modulus of Rigidity 44.1 GPa6400 ksi
Poissons Ratio 0.330.33Calculated
Machinability 92 %92 %
Forgeability 75 %75 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000460 ohm-cm0.00000460 ohm-cm37% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.7 µm/m-°C
@Temperature 20.0 - 300 °C
10.4 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 13.3 W/m-K92.0 BTU-in/hr-ft²-°F
Melting Point 988 - 1030 °C1810 - 1880 °F
Solidus 988 °C1810 °F
Liquidus 1030 °C1880 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 85.5 - 87.5 %85.5 - 87.5 %
Iron, Fe <= 0.30 %<= 0.30 %
Lead, Pb <= 0.090 %<= 0.090 %
Nickel, Ni <= 0.30 %<= 0.30 %
Phosphorus, P <= 0.10 %<= 0.10 %
Tellurium, Te 0.30 - 0.90 %0.30 - 0.90 %
Tin, Sn <= 0.30 %<= 0.30 %
Zinc, Zn <= 14.5 %<= 14.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC49100x1 / 292059

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.