MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Hytrel® 4039 TPC Polyester Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 40 Shore D High Performance Polyester Elastomer with high flow for injection molding

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccISO 1183
Melt Density 1.10 g/cc
Water Absorption 0.70 %
@Time 86400 sec
Sim. to ISO 62
 0.70 %
@Thickness 2.00 mm
Sim. to ISO 62
Moisture Absorption 0.300 %
@Thickness 2.00 mm
Sim. to ISO 62
Water Vapor Transmission 900 g/m²/day
@Thickness 0.0250 mm
DIS 15106-1/-2
Linear Mold Shrinkage, Flow 0.010 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0090 cm/cmISO 294-4, 2577
Melt Flow 22 g/10 min
@Load 2.16 kg,
Temperature 220 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 33ISO 48-4 / ISO 868
 37ISO 868
Tensile Strength, Yield 3.20 MPa
@Strain 10 %
ISO 527-1/-2
50% Modulus 6.70 MPa
@Strain 50 %
ISO 527-1/-2
Flexural Modulus 45.0 MPaISO 178
Izod Impact, Notched (ISO) NB
@Temperature 23.0 °C
ISO 180/1A
 NB
@Temperature -40.0 °C
ISO 180/1A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
 NB
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched NB
@Temperature 23.0 °C
ISO 179/1eA
 NB
@Temperature -30.0 °C
ISO 179/1eA
 NB
@Temperature -40.0 °C
ISO 179/1eA
Tear Strength 100 kN/mnormal; ISO 34-1
 100 kN/mparallel; ISO 34-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.00e+10 ohm-cmIEC 62631-3-1
Surface Resistance 3.00e+14 ohmIEC 62631-3-2
Dielectric Constant 4.7
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.8
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 18.0 kV/mmIEC 60243-1
Dissipation Factor 0.013
@Frequency 100 Hz
IEC 62631-2-1
 0.020
@Frequency 1e+6 Hz
IEC 62631-2-1
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 220 µm/m-°CISO 11359-1/-2
 280 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 200 µm/m-°CISO 11359-1/-2
 280 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
Melting Point 193 °C10°C/min; ISO 11357-1/-3
Brittleness Temperature -96.0 °CISO 974
Glass Transition Temp, Tg -50.0 °C10°C/min; ISO 11357-1/-3
Flammability, UL94 HB
@Thickness 1.50 mm
IEC 60695-11-10
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
Oxygen Index 20 %ISO 4589-1/-2
 
Processing PropertiesOriginal ValueComments
Melt Temperature 215 °COptimum
 210 - 225 °C
 225 °COptimum
 220 - 250 °C
Mold Temperature 30.0 - 40.0 °C
 40.0 °COptimum
Drying Temperature 100 °C
 90.0 - 110 °C
Dry Time 2.00 - 3.00 hourDehumidified Dryer
 2.00 - 3.00 hourDehumidified Dryer
Moisture Content <= 0.060 %
 <= 0.080 %
 
Descriptive Properties
Drying Recommended?yes
Emission of organic compounds µgC/g10VDA 277
FMVSS ClassBISO 3795 (FMVSS 302)
Odor Class4VDA 270
PolymerTPC
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDSX5172c / 295965

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.