MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC ULTEM™ Resin MD130 Polyetherimide (PEI) (Europe)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant.

Features: Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,High Heat Resistance,Good dimensional stability,Transparent

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccASTM D792
Density 1.27 g/cc0.0459 lb/in³ISO 1183
Water Absorption 0.25 %
@Time 86400 sec
0.25 %
@Time 24.0 hour
ASTM D570
Moisture Absorption 0.0100 - 0.0200 %0.0100 - 0.0200 %Extrusion Blow Molding
 0.0200 %0.0200 %Injection Molding
 0.700 %0.700 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.25 %1.25 %ASTM D570
 1.25 %1.25 %ISO 62-1
Viscosity 13 cP
@Load 5.00 kg,
Temperature 360 °C
13 cP
@Load 11.0 lb,
Temperature 680 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inSABIC method
 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 9.0 g/10 min
@Load 6.60 kg,
Temperature 337 °C
9.0 g/10 min
@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 140 MPa20300 psiH358/30; ISO 2039-1
Tensile Strength at Break 85.0 MPa12300 psi50 mm/min; ISO 527
 90.0 MPa13100 psi5 mm/min; ASTM D638
Tensile Strength, Yield 105 MPa15200 psi50 mm/min; ISO 527
 110 MPa16000 psi5 mm/min; ASTM D638
Elongation at Break 60 %60 %5 mm/min; ASTM D638
 60 %60 %50 mm/min; ISO 527
Elongation at Yield 6.0 %6.0 %50 mm/min; ISO 527
 7.0 %7.0 %5 mm/min; ASTM D638
Tensile Modulus 3.20 GPa464 ksi1 mm/min; ISO 527
 3.58 GPa519 ksi5 mm/min; ASTM D638
Flexural Strength 160 MPa23200 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
 160 MPa23200 psiyield, 2 mm/min; ISO 178
 165 MPa23900 psiyld, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 3.30 GPa479 ksi2 mm/min; ISO 178
 3.51 GPa509 ksi2.6 mm/min, 100 mm span; ASTM D790
 3.55 GPa515 ksi1.3 mm/min, 50 mm span; ASTM D790
Poissons Ratio 0.300.30ASTM E132
Izod Impact Notched 53.0 J39.1 ft-lbASTM D256
 55.0 J
@Temperature -30.0 °C
40.6 ft-lb
@Temperature -22.0 °F
ASTM D256
 1335 J
@Thickness 3.20 mm
984.6 ft-lb
@Thickness 0.126 in
reverse notched; ASTM D256
Izod Impact, Unnotched 13.35 J/cm25.01 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NBNB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
80*10*4; ISO 180/1U
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 1.00 J/cm²4.76 ft-lb/in²ISO 179/2C
 0.400 J/cm²
@Temperature -30.0 °C
1.90 ft-lb/in²
@Temperature -22.0 °F
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Gardner Impact 36.0 J26.6 ft-lbASTM D3029
Dart Drop, Total Energy 38.0 J28.0 ft-lbASTM D3763
Taber Abrasion, mg/1000 Cycles 1010CS-17, 1 kg; SABIC method
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
 1.00e+17 ohm-cm1.00e+17 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
IEC 60250
 2.9
@Frequency 50.0 - 60.0 Hz
2.9
@Frequency 50.0 - 60.0 Hz
IEC 60250
 3.15
@Frequency 1000 Hz
3.15
@Frequency 1000 Hz
ASTM D150
 3.15
@Frequency 100 Hz
3.15
@Frequency 100 Hz
ASTM D150
Dielectric Strength  16.0 kV/mm
@Thickness 3.20 mm
406 kV/in
@Thickness 0.126 in
in oil; IEC 60243-1
 19.6 kV/mm
@Thickness 3.20 mm
498 kV/in
@Thickness 0.126 in
in oil; ASTM D149
 25.0 kV/mm
@Thickness 1.60 mm
635 kV/in
@Thickness 0.0630 in
in oil; IEC 60243-1
 27.9 kV/mm
@Thickness 1.60 mm
709 kV/in
@Thickness 0.0630 in
in oil; ASTM D149
 32.7 kV/mm
@Thickness 1.60 mm
831 kV/in
@Thickness 0.0630 in
in air; ASTM D149
 33.0 kV/mm
@Thickness 0.800 mm
838 kV/in
@Thickness 0.0315 in
in oil; IEC 60243-1
Dissipation Factor  0.00050
@Frequency 50.0 - 60.0 Hz
0.00050
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0012
@Frequency 1000 Hz
0.0012
@Frequency 1000 Hz
ASTM D150
 0.0015
@Frequency 100 Hz
0.0015
@Frequency 100 Hz
ASTM D150
 0.0025
@Frequency 2.45e+9 Hz
0.0025
@Frequency 2.45e+9 Hz
ASTM D150
 0.0025
@Frequency 2.45e+9 Hz
0.0025
@Frequency 2.45e+9 Hz
IEC 60250
 0.0060
@Frequency 1e+6 Hz
0.0060
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 100 V100 VIEC 60112
 150 V150 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  50.0 µm/m-°C
@Temperature 23.0 - 150 °C
27.8 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
 55.8 µm/m-°C
@Temperature -20.0 - 150 °C
31.0 µin/in-°F
@Temperature -4.00 - 302 °F
ASTM E831
CTE, linear, Transverse to Flow  50.0 µm/m-°C
@Temperature 23.0 - 150 °C
27.8 µin/in-°F
@Temperature 73.4 - 302 °F
ISO 11359-2
 54.0 µm/m-°C
@Temperature -20.0 - 150 °C
30.0 µin/in-°F
@Temperature -4.00 - 302 °F
ASTM E831
Thermal Conductivity 0.220 W/m-K1.53 BTU-in/hr-ft²-°FASTM C177
 0.240 W/m-K1.67 BTU-in/hr-ft²-°FISO 8302
Hot Ball Pressure Test 125 °C257 °FPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °FEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FEdgew 120*10*4 sp=100mm; ISO 75/Ae
 208 °C
@Thickness 3.20 mm
406 °F
@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 211 °C412 °FRate B/50; ISO 306
 212 °C414 °FRate B/120; ISO 306
 215 °C419 °FRate A/50; ISO 306
 218 °C424 °FRate B/50; ASTM D1525
Oxygen Index 47 %47 %ISO 4589
Glow Wire Flammability Index 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 345 - 400 °C653 - 752 °F
Zone 1 325 - 350 °C617 - 662 °FExtrusion Blow Molding
Zone 2 330 - 355 °C626 - 671 °FExtrusion Blow Molding
 340 - 400 °C644 - 752 °F
Zone 3 330 - 355 °C626 - 671 °FExtrusion Blow Molding
 345 - 400 °C653 - 752 °F
Zone 4 330 - 355 °C626 - 671 °FExtrusion Blow Molding
Zone 5 330 - 355 °C626 - 671 °F
Die Temperature 325 - 355 °C617 - 671 °FExtrusion Blow Molding
Melt Temperature 320 - 355 °C608 - 671 °FExtrusion Blow Molding
 350 - 400 °C662 - 752 °FInjection Molding
Head Temperature 330 - 355 °C626 - 671 °FZone 6 - Top Temperature
 330 - 355 °C626 - 671 °FZone 7 - Bottom Temperature
Mold Temperature 65.0 - 175 °C149 - 347 °F
 135 - 165 °C275 - 329 °F
Drying Temperature 140 - 150 °C284 - 302 °FExtrusion Blow Molding
 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
 4.00 - 6.00 hour4.00 - 6.00 hourExtrusion Blow Molding
 24.0 hour24.0 hourCumulative; Injection Molding
 24.0 hour24.0 hourCumulative; Extrusion Blow Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 10 - 70 rpm10 - 70 rpm
 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82739 / 290686

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.