MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Huber Martifin® OL-005 Aluminum Hydroxide
Categories: Ceramic; Oxide; Aluminum Oxide; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Martifin® OL-005 aluminum hydroxide is pumpable aqueous suspension (slurry) of highly dispersed aluminum hydroxide for the paper and board industry, manufacturers of dispersion paints; flame retardant filler for aqueous binder systems, produced in Bergheim, Germany.

Information provided by J.M. Huber Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.66 g/cc1.66 g/cc
 2.40 g/cc2.40 g/ccData of solid
Particle Size 99.4 µm99.4 µmd50, laser diffraction
pH 7.5 - 9.07.5 - 9.0
Specific Surface Area 4.0 - 6.0 m²/g4.0 - 6.0 m²/gBET
Viscosity 67 - 69 cP67 - 69 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Mohs 2.0 - 3.02.0 - 3.0
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.581.58
 
Descriptive Properties
Al(OH)367-69%
FunctionalitySmoke Suppression
Market/Application: IndustrialPaper
Solubility in water0.001520°C, pH 7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

EHUBER720 / 300826

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.