MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) KetaSpire® KT-880 FW30 PEEK
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: KetaSpire® KT-880 FW30 is a polyetheretherketone (PEEK) compound with higher flow than KetaSpire® KT-820 SL30, making it more suitable for injection molding applications. It is designed to deliver a balance of excellent mechanical properties, wear resistance and low coefficient of friction in both dry and externally lubricated applications. The resin is formulated with anti-friction/anti-wear additive system comprised of carbon fiber and polytetrafluoroethylene (PTFE).

KetaSpire® PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, ease of melt processing, high purity, and excellent chemical resistance to organics, acids, and bases.

These properties make it well-suited for applications in transportation, electronics, chemical processing, and industrial uses including oil and gas exploration and production. The resin is black in color in its natural state.

Applications: Aircraft Applications; Connectors; Dental Applications; Electrical/Electronic Applications; Film; Hospital Goods; Industrial Applications; Medical Devices; Medical/Healthcare Applications; Oil/Gas Applications; Pump Parts; Seals; Surgical Instruments

Features: Autoclave Sterilizable; Chemical Resistant; E-beam Sterilizable; Ethylene Oxide Sterilizable; Fatigue Resistant; Flame Retardant; Good Dimensional Stability; Good Sterilizability; Heat Sterilizable; High Flow; High Heat Resistance; High Stiffness; High Strength; Radiation (Gamma) Resistant; Radiation Sterilizable; Steam Resistant; Steam Sterilizable

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.45 g/ccISO 1183
Viscosity 150 cP
@Shear Rate 1000 1/s,
Temperature 400 °C
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.00012 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0055 cm/cmISO 294-4
Melt Flow 50 g/10 min
@Load 5.00 kg,
Temperature 400 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 99ASTM D785
Tensile Strength at Break 180 MPaISO 527-2
Tensile Strength 194 MPaASTM D638
Elongation at Break 1.7 %ISO 527-2
 1.8 %ASTM D638
Tensile Modulus 13500 MPaASTM D638
 16000 MPaISO 527-2
Flexural Strength 260 MPaISO 178
 280 MPaASTM D790
Flexural Modulus 13200 MPaISO 178
 13500 MPaASTM D790
Compressive Strength 138 MPaASTM D695
Shear Strength 83.0 MPaASTM D732
Izod Impact, Notched 68.0 J/mASTM D256
Izod Impact, Unnotched 530 J/mASTM D256
Izod Impact, Notched (ISO) 7.00 kJ/m²ISO 180
Coefficient of Friction 0.28ASTM D1894
K (wear) Factor 46.0 x 10-8 mm³/N-M
@Pressure 0.220 MPa
4.1 m/sec; ASTM D3702
 
Thermal PropertiesOriginal ValueComments
Melting Point 343 °CISO 11357-3
Glass Transition Temp, Tg 147 °CISO 11357-2
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 365 °C
Middle Barrel Temperature 370 °C
Front Barrel Temperature 375 °C
Nozzle Temperature 380 °C
Mold Temperature 175 - 205 °C
Drying Temperature 150 °C
@Time 14400 sec
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
Injection RateFast
ProcessingInjection Molding; Machining; Profile Extrusion
Screw Compression Ratio2.5:1.0 to 3.5:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4337 / 280137

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.