MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ChenGuang FPM 2461 Fluoroelastomer Terpolymer Gum
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer

Material Notes: Molecular formula: -{-(CF2-CH2)65-(CF2-CF2)20-[CF2-CF(CF3)]15-}n--

Properties:

  • Excellent resistance to high temperature
  • Working for long period under 275°C.
  • Working for short period at 320°C.
  • Excellent resistance to chemical mediums. Good stability against organic liquid(oils, fuels, solvents, hydraulic oils, etc.),inorganic acids, highly-concentrated H2O2 and other oxidants. Much better than other rubbers
  • Not good resistance to M.W. ketones, esters, some ethers, NH3,NH4+,HF
  • Good mechanical properties, insulating properties, corrosion resistance
  • Common cold resistance
  • Brittle point -35°C ~-50°C ,various with formulation and thickness of the products; the thicker, the brittle point higher.
Applications: Wildly used in aviation, automobile, petroleum, and chemical industries, etc. as sealing material, to resist high temperature, corrosion, oils(especially di-ester oils, silicate ester, etc.).Usually be made into sealing rings, sealing bowls, sealing tubes, and so on. Besides, used in fabric coating to resist heat and /or corrosion.

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.84 - 1.88 g/cc1.84 - 1.88 g/ccGum
Viscosity 20 - 40 cP
@Temperature 121 °C
20 - 40 cP
@Temperature 250 °F
ML(1+10), Gum
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break >= 8.00 MPa>= 1160 psiVulcanized Elastomer
Elongation at Break >= 230 %>= 230 %Vulcanized Elastomer
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %Gum
 
Component Elements PropertiesMetricEnglishComments
Fluorine, F 68.2 - 69 %68.2 - 69 %Gum
 
Descriptive Properties
Colorwhite or yellowish slabs
Fluid Resistance0.061# jet fuel, Vulcanized Elastomer
Thermolysis temperature>320°CGum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGU005 / 255604

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.