MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin FP5140HF Polyphenylene Ether + PS (PPE+PS)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ FP5140HF resin is an impact modified, unreinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This injection moldable grade contains non-brominated, non-chlorinated flame retardant with a UL94 flame rating of V1 at 1.5mm. NORYL FP5140HF resin was designed to have very good dimensional stability with high flow and exhibits good rheological properties, high heat resistance, hydrolysis resistance, and very low density. The combination of these properties makes this material an excellent candidate for Flat Panel TV enclosure applications.

Features: Hydrolytic Stability,Low Creep Sensitivity,Flame Retardant,Thin Wall,Non-Halogenated,Non-Chlorinated,Non-Brominated,Low Warpage,High Flow,Good Processability

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.11 g/ccASTM D792
Density 1.11 g/ccISO 1183
Moisture Absorption 0.0500 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.18 %ISO 62-1
Viscosity 17 cP
@Load 1.20 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
 48 cP
@Load 2.16 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
SABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 44.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 48.0 MPa50 mm/min; ISO 527
Elongation at Break 21.4 %50 mm/min; ISO 527
Elongation at Yield 2.7 %50 mm/min; ISO 527
Tensile Modulus 2530 MPa1 mm/min; ISO 527
 2940 MPa50 mm/min; ASTM D638
Flexural Strength 80.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2450 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 7.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 83.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 83.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 77.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 77.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 78.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 97.0 °CRate B/50; ASTM D1525
 97.0 °CRate B/50; ISO 306
 100 °CRate B/120; ISO 306
UL RTI, Electrical 65.0 °CUL 746B
UL RTI, Mechanical with Impact 65.0 °CUL 746B
UL RTI, Mechanical without Impact 65.0 °CUL 746B
Flammability, UL94 V-1
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 240 - 270 °C
Zone 2 230 - 260 °C
Zone 3 250 - 285 °C
Melt Temperature 250 - 285 °CInjection Molding
Mold Temperature 40.0 - 65.0 °C
Drying Temperature 70.0 - 80.0 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82303 / 290250

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.