MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SABIC GELOY™ XP4034 ASA (Asia)
Categories: Polymer; Thermoplastic; ASA Polymer

Material Notes: PC/ASA. Excellent weatherability.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
Water Absorption 0.25 %0.25 %24 hours; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 24 g/10 min
@Load 3.80 kg,
Temperature 280 °C
24 g/10 min
@Load 8.38 lb,
Temperature 536 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 110110ASTM D785
Tensile Strength, Yield 62.0 MPa8990 psi50 mm/min; ASTM D638
Elongation at Break 25 %25 %50 mm/min; ASTM D638
Flexural Yield Strength 88.0 MPa12800 psi1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.51 GPa364 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 3.20 J/cm5.99 ft-lb/inASTM D256
 0.800 J/cm
@Temperature -30.0 °C
1.50 ft-lb/in
@Temperature -22.0 °F
ASTM D256
Dart Drop, Total Energy 47.0 J34.7 ft-lbASTM D3763
 30.0 J
@Temperature -30.0 °C
22.1 ft-lb
@Temperature -22.0 °F
ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 72.0 µm/m-°C
@Temperature -20.0 - 150 °C
40.0 µin/in-°F
@Temperature -4.00 - 302 °F
ASTM E831
CTE, linear, Transverse to Flow 72.0 µm/m-°C
@Temperature -20.0 - 150 °C
40.0 µin/in-°F
@Temperature -4.00 - 302 °F
ASTM E831
Thermal Conductivity 0.250 W/m-K1.74 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 115 °C
@Thickness 3.20 mm
239 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C
@Thickness 6.40 mm
219 °F
@Thickness 0.252 in
unannealed; ASTM D648
 
Optical PropertiesMetricEnglishComments
Gloss 94 %94 %60°; ASTM D523
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 245 - 265 °C473 - 509 °FInjection Molding
Zone 1 225 - 240 °C437 - 464 °FSheet Extrusion
 240 - 255 °C464 - 491 °F
Zone 2 240 - 250 °C464 - 482 °FSheet Extrusion
 245 - 260 °C473 - 500 °F
Zone 3 250 - 260 °C482 - 500 °FSheet Extrusion
 250 - 265 °C482 - 509 °F
Zone 4 260 - 270 °C500 - 518 °FSheet Extrusion
Adapter Temperature 260 - 270 °C500 - 518 °FSheet Extrusion
Die Temperature 260 - 270 °C500 - 518 °FSheet Extrusion
Melt Temperature 260 - 275 °C500 - 527 °F
 260 - 280 °C500 - 536 °F
Mold Temperature 55.0 - 70.0 °C131 - 158 °F
Roll Temperature 75.0 - 90.0 °C167 - 194 °FRoll Stack Temp - Bottom
 95.0 - 110 °C203 - 230 °FRoll Stack Temp - Middle
 100 - 120 °C212 - 248 °FRoll Stack Temp - Top
Drying Temperature 90.0 - 100 °C194 - 212 °FSheet Extrusion
 95.0 - 105 °C203 - 221 °FInjection Molding
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hourInjection Molding
 3.00 - 4.00 hour3.00 - 4.00 hourSheet Extrusion
 8.00 hour8.00 hourCumulative; Sheet Extrusion
 8.00 hour8.00 hourCumulative; Injection Molding
Moisture Content 0.040 %0.040 %
 >= 0.040 %>= 0.040 %
Back Pressure 0.300 - 1.00 MPa43.5 - 145 psi
Shot Size 40 - 80 %40 - 80 %
Vent Depth 0.00380 - 0.00760 cm0.00150 - 0.00299 in
Screw Speed 30 - 80 rpm30 - 80 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABI10151 / 243618

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.