MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ STAT-KON™ Compound DD0001 Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DD0001 compound is based on Polycarbonate (PC) resin containing conductive carbon powder. Added features of this grade include: Electrically Conductive, Non-Brominated, Non-Chlorinated Flame Retardant.

Features: Flame Retardant,Non-Chlorinated,Non-Brominated,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.28 g/cc0.0462 lb/in³ASTM D792
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.100 %0.100 %23°C/50% RH/24 hrs; ASTM D570
 0.140 %0.140 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0039 cm/cm0.0039 in/in24hrs; ISO 294
 0.0040 cm/cm0.0040 in/in24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 cm/cm0.0040 in/in24hrs; ASTM D955
 0.0040 cm/cm0.0040 in/in24hrs; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 64.0 MPa9280 psiASTM D638
 64.0 MPa9280 psiISO 527
Elongation at Break 3.2 %3.2 %ISO 527
 3.6 %3.6 %ASTM D638
Tensile Modulus 3.45 GPa500 ksi50 mm/min; ASTM D638
 3.75 GPa544 ksi1 mm/min; ISO 527
Flexural Strength 103 MPa14900 psiISO 178
 116 MPa16800 psiASTM D790
Flexural Modulus 3.51 GPa509 ksiASTM D790
 3.52 GPa511 ksiISO 178
Izod Impact Notched 23.0 J17.0 ft-lbASTM D256
Izod Impact, Unnotched 5.50 J/cm10.3 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 2.00 kJ/m²0.952 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 36.0 kJ/m²17.1 ft-lb/in²80*10*4; ISO 180/1U
Dart Drop, Total Energy 1.00 J0.738 ft-lbpeak; ASTM D3763
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 100 - 1.00e+6 ohm100 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  52.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
29.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 52.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
29.0 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  52.3 µm/m-°C
@Temperature -40.0 - 40.0 °C
29.1 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 52.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
29.1 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 88.0 °C190 °FFlatw 80*10*4 sp=64mm; ISO 75/Bf
 86.0 °C
@Thickness 3.20 mm
187 °F
@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C180 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 82.0 °C
@Thickness 3.20 mm
180 °F
@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 V-1
@Thickness 2.30 mm
V-1
@Thickness 0.0906 in
UL 94
 
Processing PropertiesMetricEnglishComments
Zone 2 255 - 265 °C491 - 509 °F
Zone 3 260 - 270 °C500 - 518 °F
Melt Temperature 255 - 290 °C491 - 554 °FInjection Molding
Mold Temperature 40.0 - 65.0 °C104 - 149 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH81183 / 289130

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.