MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
TBA ECP 2200 Anti Static Dissipative Colorable Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade; Polypropylene, Molded

Material Notes: An injection molding compound utilizing a special non-migratory additive system to give a permanently anti static dissipative material. The material is specially designed for applications requiring static control such as electronic safe handling areas and hazardous environments.

Applications:

  • Production aids for the electronics industry (eg storage boxes bins etc)
  • Plastic parts for hazardous environments
  • Audio/Hi-Fi accessories
  • Static dissipating equipment housing

Information provided by TBA Protective Solutions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.930 g/cc
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 28.0 MPaISO 527
Elongation at Break 200 %ISO 527
Tensile Modulus 1600 MPaISO 527
Flexural Modulus 1400 MPaISO 178
Izod Impact, Notched NBBS 2873
Charpy Impact Unnotched NB
Charpy Impact, Notched NB
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 1.00e+8 ohmDIN 53482
Static Decay <= 0.25 sec5000/50V; FTMS-101C
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
Shrinkage 1.6 - 2.0 %
 
Processing PropertiesOriginal ValueComments
Processing Temperature 200 - 230 °CCylinder
Mold Temperature 25.0 - 50.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PTBA017 / 281495

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.