LNP STAT-KON LX04420C compound is based on Polyetheretherketone (PEEK) resin containing carbon fiber. Added features of this grade include: LNP Clean Compounding Technology, Electrically Conductive, Dimensional Stability. Features: LNP Clean Compound Technology,High Stiffness,Light-weight Structural,High Heat Resistance,Super Strong (Carbon Fiber Filled),Good dimensional stability,Electrically Conductive Information provided by SABIC |