MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper Alloy, UNS C18160, TR08 Temper; Flat Products , Rod & Bar
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Precipitation or Spinodal Heat-treated, Spring and Thermal Stress Relieved

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked; Good Suitability – Gas Shielded Arc Welding; Fair Suitability – Spot Weld, Seam Weld, Butt Weld, Capacity for Being Hot Formed

Typical Uses: Automotive Electronic Connectors; Connectors, Automotive; Connectors, Terminals, Contact Springs, Fuse Clamps, Circuit breaker components

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.86 g/cc0.320 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 160 - 190
@Load 3.00 kg
160 - 190
@Load 6.62 lb
Tensile Strength 558 MPa81000 psiTypical
 538 - 621 MPa78000 - 90000 psi
Tensile Strength, Yield >= 496 MPa>= 72000 psi
Elongation at Break 8.0 %8.0 %
Tensile Modulus 137 GPa19900 ksi
Machinability 20 %20 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000200 ohm-cm0.00000200 ohm-cm86% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 - 300 °C
10.0 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 27.5 W/m-K191 BTU-in/hr-ft²-°F
Melting Point 1070 - 1080 °C1958 - 1976 °F
Solidus 1070 °C1958 °F
Liquidus 1080 °C1976 °F
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 0.20 - 1.2 %0.20 - 1.2 %
Copper, Cu 98.4 - 99.8 %98.4 - 99.8 %As Balance
Iron, Fe <= 0.10 %<= 0.10 %
Silicon, Si <= 0.10 %<= 0.10 %
Zirconium, Zr 0.050 - 0.25 %0.050 - 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC18160x3 / 291650

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.