Product Description: Polyester flock is manufactured from Terephthalate ester fibers. Polyester flock offers the following benefits: Excellent abrasion resistance; Excellent dimension stability; Low resin & solvent demand; Excellent UV resistance; Excellent resistance to mildew, oil, acids and many other chemicals.Information provided by Akrochem Corporation |