MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultraform® N 2720 M210 AT POM, 10% Mineral Reinforced
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Mineral Filled

Material Notes: Product Description: Ultraform® N 2720 M210 AT is a 10% mineral reinforced injection molding POM grade with good wear properties for low-warpage parts with enhanced stiffness, strength and hardness. Typical applications include conveyor belts and transportation systems.

Availability: North America

Filler/Reinforcement: Mineral, 10% Filler by Weight

Features: Good Hardness; Good Stiffness; Good Strength; Low Warpage; Wear Resistant

Use: Belts/Belt Repair

Agency Ratings: EC 1907/2006 (REACH)

RoSH Compliance: RoSH Compliant

Processing Method: Injection Molding

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³ISO 1183
Water Absorption 0.20 %0.20 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 0.80 %0.80 %ISO 62
Maximum Moisture Content 0.150.15
Linear Mold Shrinkage, Flow 0.017 cm/cm0.017 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/inISO 294-4
Melt Flow 7.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 63.0 MPa9140 psiISO 527-2
Elongation at Yield 9.5 %9.5 %ISO 527-2
Tensile Modulus 3.80 GPa551 ksiISO 527-1
Charpy Impact Unnotched  9.03 J/cm²
@Temperature -30.0 °C
43.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 9.03 J/cm²
@Temperature 22.8 °C
43.0 ft-lb/in²
@Temperature 73.0 °F
ISO 179
Charpy Impact, Notched  0.357 J/cm²
@Temperature -30.0 °C
1.70 ft-lb/in²
@Temperature -22.0 °F
ISO 179
 0.357 J/cm²
@Temperature 22.8 °C
1.70 ft-lb/in²
@Temperature 73.0 °F
ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 86.6 kV/mm2200 kV/inIEC 60243-1
Dissipation Factor 0.0060
@Frequency 1e+6 Hz
0.0060
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 79.2 µm/m-°C44.0 µin/in-°FISO 11359-2
Melting Point 166 °C331 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 115 °C239 °FUnannealed; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 230 °C374 - 446 °F
Mold Temperature 60.0 - 120 °C140 - 248 °F
Drying Temperature 80.0 - 110 °C176 - 230 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Injection Pressure 3.50 - 17.0 MPa508 - 2470 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2131 / 310824

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.