MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
KLJ Group KANATOL 8080 Primary plasticizer for PVC and PVC copolymers
Categories: Fluid

Material Notes: Properties: Kanatol-8080 is transparent liquid with stability and is soluble in most organics solvent. Kanatol-8080 is used in a lot of European countries in application where human body is directly in contact with material like toys, nappy, medical material, artificial leather, water pipe. Kanatol-8080 is not limited as carcinogen DOP. You can add your products as NON CARCINOGEN PRODUCT. It has different structure than phthalic based plasticizers. As a result of this migration is lower. The materials, which are made with K-8080, are more resistant to most of hydrocarbons. It has lower flexibility because of its structure and this decreases fragility. It can lubricate itself because of structural characteristics. Preparing plastisol with K-8080 consumes shorter time and less energy. K-8080 can be replaced with DINP/DIDP because of lower volatile losses. Preferable plasticizer for producing cable with excellent electrical specialties.

Application: KANATOL-8080 is a primary plasticizes for soft PVC products and is recommended to be used in high –temperature cable and wire. KANATOL-8080 used in vinyl gloves, wall covering, vinyl flooring, carpet & novelties and synthetic rubber.

Chemical Name: Di-(2-ethylhexyl) 1,4 benzene di carboxylate

Molecular Formula: C 24 H38 O 4

Molecular Structure: C6 H4 -1,4-[CO 2 CH2 CH(C2 H 5 )(CH2 ) CH3 ] 2

CAS Number: 6422-86-2

EINECS NO: 229-176-9

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 - 0.986 g/cc
@Temperature 27.0 °C
ASTM-D-1045-86
Viscosity 61 - 65 cP
Molecular Weight 390 g/mol
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.50e+11 - 4.50e+11 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Boiling Point 400 °C
Flash Point >= 210 °CCOC
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.484 - 1.489
@Temperature 27.0 °C
ASTM-D-1045-86
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %ASTM-E-203
Shelf Life 24.0 Month
 
Descriptive Properties
Acidity after heat treatment0.0003ASTM-D-1045-86
Acidity as Acid<0.01%ASTM-D-1045-86
Color<20 HUASTM-D-1045-86
Content<0.10%Residual alcohol
 >99.5Ester Content, ASTM-D-1045-86
 >99.5%Plasticizing Ester, ASTM-D-1045-86
 284-290 mg KOH/gEster Value, ASTM-D-1045-86

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKLJ342 / 284363

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.