GSO MultiFibre® PP Directroving of E-glass and polypropylene fibers for the production of reinforced semi finishes and parts. The hybrid fibers have a nominal yield of1870 tex with a mass ratio of 40 % PP as matrix and 60 % glass as reinforcement. Other matrix- /reinforcement ratios on request.Information provided by Oschatz-Glas |