Compound 3756 is a 70 durometer yellow colored general purpose Buna N elastomer. It exhibits good resistance to heat and petroleum based oils. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 BF 725 EO14 EO34; 2 BG 725 EO14 EO34 EF11; 3 BG 725 EO14; 4 BG 720 A14 B14 EO14; 5 BG 720 A14 EO14 EO34 This Compound is RoHS Compliant Information provided by Pressure Seals Inc. |