MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® 3501-6 Epoxy Resin System
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: 3501-6 is an amine cured epoxy resin system supplied with unidirectional or woven carbon or glass fibers. Typical reinforcement is continuous AS4 carbon filaments. 3501-6 was developed to operate in a temperature environment of up to 350°F (177°C). AS4/3501-6 is recommended for general purpose structural applications.

Benefits and Features:

  • Service Temperature up to 350°F (177°C)
  • Damage-Resistant System
  • 350°F (177°C) Cure

Information provided by Hexcel Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.265 g/cc0.04570 lb/in³
Viscosity 400 cP400 cP
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 45.5 MPa6600 psi
Tensile Modulus 4.24 GPa615 ksi
Flexural Modulus 3.34 GPa484 ksi
Compressive Strength 1.10 MPa160 psi
 1.95 MPa283 psiShear elongation to failure
Shear Strength 48.3 MPa7000 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear  38.0 µm/m-°C
@Temperature 23.9 - 72.8 °C
21.1 µin/in-°F
@Temperature 75.0 - 163 °F
 43.9 µm/m-°C
@Temperature 71.1 - 121 °C
24.4 µin/in-°F
@Temperature 160 - 250 °F
 59.9 µm/m-°C
@Temperature 121 - 177 °C
33.3 µin/in-°F
@Temperature 250 - 350 °F
Glass Transition Temp, Tg  151 °C
@Temperature 177 °C,
Time >=21600 sec
304 °F
@Temperature 350 °F,
Time >=6.00 hour
wet
 210 °C
@Temperature 177 °C,
Time >=21600 sec
410 °F
@Temperature 350 °F,
Time >=6.00 hour
dry
 
Processing PropertiesMetricEnglishComments
Gel Time 4.00 - 10.0 min
@Temperature 177 °C
4.00 - 10.0 min
@Temperature 351 °F
Shelf Life  0.300 Month
@Temperature 21.0 °C
0.300 Month
@Temperature 69.8 °F
 4.00 Month
@Temperature 4.00 °C
4.00 Month
@Temperature 39.2 °F
 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
G1 C0.733 in-lb/in2Strain energy release rate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHEXCB9118 / 322274

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.