MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A 50H1 Black LBO 129 Nylon 66, Heat Stabilized, Flame Retardant, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized; Nylon 66, Unreinforced, Flame Retardant

Material Notes: Product Description: Ultramid® A 50H1 Black LBO 129 is an unreinforced polyamide 66 based on a non-phosphorous and non-halogenated flame retardant system, heat stabilized, for injection molding. This flame retardant grade, offers excellent filling qualities combined with good stiffness. European Railways Certifications – EN 45545-2 HL2; European Railways Certifications – EN 45545-2 HL3

Availability: North America

Additive: Flame Retardant; Heat Stabilizer

Features: Flame Retardant; Good Moldability; Good Stiffness; Halogen Free; Heat Stabilized; Low (to None) Phosphorus Content

Agency Ratings: EC 1907/2006 (REACH); EN 45545; UL QMFZ2

RoSH Compliance: RoSH Compliant

Appearance: Black; Natural Color

Forms: Pellets

Processing Method: Injection Molding

Resin ID (ISO 1043): PA66 FR(30)

Information provided by BASF Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³ISO 1183
Water Absorption 2.7 %2.7 %Equilibrium, 50% RH; ISO 62
 0.88 %
@Time 86400 sec
0.88 %
@Time 24.0 hour
ISO 62
Maximum Moisture Content 0.200.20
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 75.2 MPa10900 psiISO 527-2
Tensile Strength, Yield 80.0 MPa11600 psiISO 527-2
Elongation at Break 9.0 %9.0 %ISO 527-2
Tensile Modulus 3.80 GPa551 ksiISO 527-1
Flexural Strength 120 MPa17400 psiASTM D790
 130 MPa18900 psiISO 178
Flexural Modulus 3.70 GPa537 ksiISO 178
 3.80 GPa551 ksiASTM D790
Izod Impact, Notched (ISO) 1.57 kJ/m²0.750 ft-lb/in²ASTM D256
 2.94 kJ/m²1.40 ft-lb/in²ISO 180/A
Charpy Impact Unnotched  7.98 J/cm²
@Temperature 22.8 °C
38.0 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eU
 7.98 J/cm²
@Temperature -30.0 °C
38.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched  0.294 J/cm²
@Temperature -30.0 °C
1.40 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.315 J/cm²
@Temperature 22.8 °C
1.50 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.00e+15 ohm-cm3.00e+15 ohm-cmIEC 62631-3-1
Dielectric Constant 3.5
@Frequency 100 Hz
3.5
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength  20.9 kV/mm
@Thickness 2.00 mm
530 kV/in
@Thickness 0.0787 in
IEC 60243-1
 33.1 kV/mm
@Thickness 0.800 mm
840 kV/in
@Thickness 0.0315 in
IEC 60243-1
Dissipation Factor 0.017
@Frequency 100 Hz
0.017
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 600 V600 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °FISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 237 °C459 °FUnannealed; ISO 75-2/Bf
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FUnannealed; ISO 75-2/Af
Flammability, UL94  V-0
@Thickness 0.787 mm
V-0
@Thickness 0.0310 in
 V-0
@Thickness 3.30 mm
V-0
@Thickness 0.130 in
Oxygen Index 33 %33 %ISO 4589-2
Glow Wire Ignition Temperature  960 °C
@Thickness 0.406 mm
1760 °F
@Thickness 0.0160 in
IEC60695-2-13
 960 °C
@Thickness 0.787 mm
1760 °F
@Thickness 0.0310 in
IEC60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.787 mm
1760 °F
@Thickness 0.0310 in
IEC 60695-2-12
 960 °C
@Thickness 1.52 mm
1760 °F
@Thickness 0.0600 in
IEC 60695-2-12
 960 °C
@Thickness 2.87 mm
1760 °F
@Thickness 0.113 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 270 °C500 - 518 °F
Middle Barrel Temperature 265 - 275 °C509 - 527 °F
Front Barrel Temperature 265 - 275 °C509 - 527 °F
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
Drying Temperature 80.0 °C176 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASG2076 / 310769

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.