MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
BASF 3D Ultrafuse® PET Fused Fillament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Components: Amorphous Polyethylene Terephthalate based filament for Fused Filament Fabrication.

Product Description: Ultrafuse PET is made from a premium PET and prints as easy as PLA, but is much stronger. The filament has a large operating window for printing (temperature vs. speed), so it can be used on every 3D-printer. PET will give you outstanding printing results: a good layer adhesion, a high resolution and it is easy to handle. Ultrafuse PET can be 100% recycled, is watertight and has great colors and finish.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.329 g/ccPrinted Part; ISO 1183-1
Melt Flow 21.6627 g/10 min
@Load 2.16 kg,
Temperature 220 °C
ISO 1133
Storage Temperature 15.0 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 17.2 MPaZX: Upright; ISO 527
 33.4 MPaXY: Flat; ISO 527
Elongation at Break 1.1 %ZX: Upright; ISO 527
 2.7 %XY: Flat; ISO 527
Modulus of Elasticity 1.665 GPaYoung's, ZX: Upright; ISO 527
 1.933 GPaYoung's, XY: Flat; ISO 527
Flexural Strength 54.4 MPaZX: Upright; ISO 178
 66.7 MPaXY: Flat; ISO 178
 76.1 MPaXZ: On its edge; ISO 178
Flexural Modulus 1826 MPaZX: Upright; ISO 178
 1840 MPaXZ: On its edge; ISO 178
 2063 MPaXY: Flat; ISO 178
Flexural Strain at Break 3.0 %ZX: Upright; ISO 178
 4.6 %XY: Flat; ISO 178
 4.6 %XZ: On its edge; ISO 178
Izod Impact, Notched (ISO) 1.80 kJ/m²ZX: Upright; ISO 180
 1.90 kJ/m²XZ: On its edge; ISO 180
 2.10 kJ/m²XY: Flat; ISO 180
Izod Impact, Unnotched (ISO) 4.10 kJ/m²ZX: Upright; ISO 180
 7.70 kJ/m²XZ: On its edge; ISO 180
 12.3 kJ/m²XY: Flat; ISO 180
Charpy Impact Unnotched 4.60 kJ/m²ZX: Upright; ISO 179-2
 9.70 kJ/m²XZ: On its edge; ISO 179-2
 18.4 kJ/m²XY: Flat; ISO 179-2
Charpy Impact, Notched 1.20 kJ/m²ZX: Upright; ISO 179-2
 1.40 kJ/m²XZ: On its edge; ISO 179-2
 1.60 kJ/m²XY: Flat; ISO 179-2
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 63.0 °CISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 61.0 °CISO 75-2
Glass Transition Temp, Tg 71.0 °CISO 11357-2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 60.0 - 80.0 °CBed, Bed Material: Glass
Nozzle Temperature 210 - 230 °C
Drying Temperature 60.0 °Cin a hot air dryer or vacuum oven
Dry Time 4.00 - 16.0 hour
Shelf Life 12.0 Month
 
Descriptive Properties
Nozzle Diameter=0.4 mm
Print speed40-80 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASF3D002 / 312243

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.