Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.19 g/cc | 1.19 g/cc |
Density | 1.19 g/cc | 0.0430 lb/in³ |
Moisture Absorption | 0.0200 % | 0.0200 % |
| 0.150 % | 0.150 % |
Water Absorption at Saturation | 0.40 % | 0.40 % |
Viscosity | 15 cP @Load 1.20 kg, Temperature 300 °C | 15 cP @Load 2.65 lb, Temperature 572 °F |
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm | 0.0040 - 0.0080 in/in @Thickness 0.126 in |
Melt Flow | 16 g/10 min @Load 1.20 kg, Temperature 300 °C | 16 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Mechanical Properties | Metric | English | Comments |
---|
Tensile Strength at Break | 57.0 MPa | 8270 psi |
| 59.0 MPa | 8560 psi |
Tensile Strength, Yield | 56.0 MPa | 8120 psi |
| 58.0 MPa | 8410 psi |
Elongation at Break | 108 % | 108 % |
| 115 % | 115 % |
Elongation at Yield | 6.0 % | 6.0 % |
| 6.0 % | 6.0 % |
Tensile Modulus | 2.00 GPa | 290 ksi |
| 2.10 GPa | 305 ksi |
Flexural Strength | 87.0 MPa | 12600 psi |
| 92.0 MPa | 13300 psi |
Flexural Modulus | 2.10 GPa | 305 ksi |
| 2.40 GPa | 348 ksi |
Izod Impact Notched | 785 J | 579 ft-lb |
| 380 J @Temperature -40.0 °C | 280 ft-lb @Temperature -40.0 °F |
| 655 J @Temperature -30.0 °C | 483 ft-lb @Temperature -22.0 °F |
Izod Impact, Notched (ISO) | 65.0 kJ/m² | 30.9 ft-lb/in² |
| 30.0 kJ/m² @Temperature -30.0 °C | 14.3 ft-lb/in² @Temperature -22.0 °F |
Izod Impact, Unnotched (ISO) | NB | NB |
| NB @Temperature -30.0 °C | NB @Temperature -22.0 °F |
Charpy Impact Unnotched | NB | NB |
| NB @Temperature -30.0 °C | NB @Temperature -22.0 °F |
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² |
| 3.50 J/cm² @Temperature -30.0 °C | 16.7 ft-lb/in² @Temperature -22.0 °F |
Dart Drop, Total Energy | 67.0 J | 49.4 ft-lb |
|
Electrical Properties | Metric | English | Comments |
---|
Comparative Tracking Index | 175 - 250 V | 175 - 250 V |
Hot Wire Ignition, HWI | 15 - 30 sec @Thickness >=0.750 mm | 15 - 30 sec @Thickness >=0.0295 in |
| 30 - 60 sec @Thickness >=3.00 mm | 30 - 60 sec @Thickness >=0.118 in |
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness >=0.750 mm | 60 - 120 arcs @Thickness >=0.0295 in |
| >= 120 arcs @Thickness >=3.00 mm | >= 120 arcs @Thickness >=0.118 in |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear, Parallel to Flow | 61.0 µm/m-°C @Temperature -40.0 - 40.0 °C | 33.9 µin/in-°F @Temperature -40.0 - 104 °F |
| 61.0 µm/m-°C @Temperature -40.0 - 40.0 °C | 33.9 µin/in-°F @Temperature -40.0 - 104 °F |
CTE, linear, Transverse to Flow | 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C | 34.4 µin/in-°F @Temperature -40.0 - 104 °F |
| 62.0 µm/m-°C @Temperature -40.0 - 40.0 °C | 34.4 µin/in-°F @Temperature -40.0 - 104 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 118 °C | 244 °F |
| 123 °C @Thickness 3.20 mm | 253 °F @Thickness 0.126 in |
Vicat Softening Point | 139 °C | 282 °F |
| 140 °C | 284 °F |
| 141 °C | 286 °F |
UL RTI, Electrical | 125 °C | 257 °F |
UL RTI, Mechanical with Impact | 115 °C | 239 °F |
UL RTI, Mechanical without Impact | 125 °C | 257 °F |
Flammability, UL94 | V-0 @Thickness >=1.50 mm | V-0 @Thickness >=0.0591 in |
| 5VA @Thickness >=3.00 mm | 5VA @Thickness >=0.118 in |
Glow Wire Ignition Temperature | 825 °C @Thickness 1.50 mm | 1520 °F @Thickness 0.0591 in |
| 825 °C @Thickness 3.00 mm | 1520 °F @Thickness 0.118 in |
Glow Wire Flammability Index | 960 °C @Thickness 1.50 mm | 1760 °F @Thickness 0.0591 in |
| 960 °C @Thickness 3.00 mm | 1760 °F @Thickness 0.118 in |
| 960 °C @Thickness >=1.50 mm | 1760 °F @Thickness >=0.0591 in |
|
Processing Properties | Metric | English | Comments |
---|
Nozzle Temperature | 290 - 310 °C | 554 - 590 °F |
Zone 2 | 280 - 305 °C | 536 - 581 °F |
Zone 3 | 295 - 315 °C | 563 - 599 °F |
Melt Temperature | 295 - 315 °C | 563 - 599 °F |
Mold Temperature | 70.0 - 95.0 °C | 158 - 203 °F |
Drying Temperature | 120 °C | 248 °F |
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour |
| 48.0 hour | 48.0 hour |
Back Pressure | 0.300 - 0.700 MPa | 43.5 - 102 psi |
Shot Size | 40 - 60 % | 40 - 60 % |
Vent Depth | 0.00250 - 0.00760 cm | 0.000984 - 0.00299 in |
Screw Speed | 40 - 70 rpm | 40 - 70 rpm |
|
Descriptive Properties |
---|
UV-light, water exposure/immersion | F1 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.