Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Additive: Flame Retardant Features: Flame Retardant; Good Flow; Good Mold Release Uses: Appliance Components; Automotive Applications; Automotive Electronics; Connectors; Electrical/Electronic Applications; Lighting Applications; Tubing; Wire & Cable Applications Forms: Granules Processing Method: Injection Molding Information provided by EMS-Grivory |